Electronics Forum | Thu Apr 08 08:34:34 EDT 2004 | Evtimov
The camera is in the head. Sorry forgot to tell you.Stefan now I do the calibration with inprint in a putty. Ken I am looking for accuracy when I calibrate the camera. Tell me more about that slug. What is it like? Where to place it? How to use it?
Electronics Forum | Wed Apr 07 20:58:50 EDT 2004 | davef
There's a variety of reports like you see on the net. Here's one: http://www.buscom.com/chem/C137N.html
Electronics Forum | Fri Apr 16 10:42:04 EDT 2004 | davef
Possibilities are: * Handling problems, like Bob L [the previous poster in this thread] mentioned. * Poor reflow recipe selection. Search the SMTnet Archives for previous discussion. [Your English is fine. Most of us "English" writers don't do any
Electronics Forum | Tue Apr 20 09:21:40 EDT 2004 | lbiggs
We use 8X10 Ziplock A/S poly bag 4 mil pink at our taping facility. We also sell as a supply. If interested or you would like more information please call Sarah Lewis at V-TEK Inc. 507-387-2039 X 148.
Electronics Forum | Thu May 27 06:47:45 EDT 2004 | Bryan Sherh
Hello All, I 'd like to have some stuffs about immersion Silver to study with.Can anybody provide some information or some articles about Immersion silver? Thanks a lot. Bryan
Electronics Forum | Thu May 27 06:48:20 EDT 2004 | Bryan Sherh
Hello All, I 'd like to have some stuffs about immersion Silver to study with.Can anybody provide some information or some articles about Immersion silver? Thanks a lot. Bryan Bryan.she@163.com
Electronics Forum | Tue Jun 08 08:27:14 EDT 2004 | michaeljm
I would like to see the report from MacDermid. We have samples of ag boards in which the underside of PCB pad has been plated between the PCB laminate and pad.
Electronics Forum | Wed Apr 21 21:13:02 EDT 2004 | davef
It's an ol'timey process. Used for wear surfaces and the like. Look here: http://www.smta.org/knowledge/proceedings_abstract.cfm?PROCEEDING_ID=846
Electronics Forum | Mon Apr 26 22:55:53 EDT 2004 | CT
Hi, I'm setting up a procedure for Moisture sensitive IC rework. Would like to understand what is the baking requirement for a board before a moisture sensitive IC can be remove from a board.
Electronics Forum | Tue Apr 27 17:28:21 EDT 2004 | vms
You can call us, we will give you some tech support free. I realize that you may not be in the USA but there is a lot of various reasons why it will not reset. You can call us if you would like 740-344-4260 Harry