Electronics Forum: solderers (Page 1126 of 2099)

Micro crack for lead free wave solder

Electronics Forum | Mon Aug 01 08:38:57 EDT 2005 | kamrant

Joseph, What is the topside temp reading of your board before reaching the pot? Do you have top-heater in your wave machine? It sounds like; you got an insufficient per-heating issue.

Micro crack for lead free wave solder

Electronics Forum | Mon Aug 01 20:02:20 EDT 2005 | Joseph

We use SAC305 and top side particular joint temp. is 110 deg C, and the terminal finish for that particular lead is pure tin. It look like hot tearing at the primary side of PTH.

Table Top Router

Electronics Forum | Wed Aug 03 09:58:16 EDT 2005 | Rob

http://www.micromat.co.uk/economy.htm We've got one of these & it's been great - whether for depanelising, making wave solder pallets, SMT flexi carriers, drilling prototype pcbs etc. Really easy to programme too.

ENIG switch contacts

Electronics Forum | Mon Aug 08 19:26:22 EDT 2005 | Tom B

That uis correct if your wanting solderable gold it should be 10-17uinches, but for coantact suchas as switches and card edge 30 is used

PCB cosmetic reject after reflow

Electronics Forum | Mon Aug 08 20:25:39 EDT 2005 | plcc

Hi Davef, I'm suspecting that too! The recipe we are using is the optimum for good soldering results. I'm checking with our supplier on the type of pcb material. Do you know the recommended material for pcb undergoing reflow, under ROsH condition?

PCB cosmetic reject after reflow

Electronics Forum | Mon Aug 08 21:34:44 EDT 2005 | davef

Jim Can you be more specific? What's going "yellow / beige" on you? * Laminate * Solder mask * Legend

PCB cosmetic reject after reflow

Electronics Forum | Mon Aug 08 22:40:49 EDT 2005 | davef

Jim Can you be more specific? What's going "yellowish" on you? * Laminate * Solder mask * Legend

kapton dots and liquid solder mask

Electronics Forum | Tue Aug 09 10:38:45 EDT 2005 | SuMoTe

Water soluable dots will wash off after reflow. A water soluable liquid mask will work as well. dots are better for defined (round)holes, whereas the liquid mask works well with odd shapes.

kapton dots and liquid solder mask

Electronics Forum | Wed Aug 10 15:09:06 EDT 2005 | pr

O.K. thanks, I'll look into it............through a rep, since all our boardhouses are in China/Taiwan. I'm seeing a pattern! thanks, pr

kapton dots and liquid solder mask

Electronics Forum | Thu Aug 18 13:11:39 EDT 2005 | jsloot

We have our board house apply a peel coat mask that can be brushed off after wave or reflow. You need to brush off while it's still warm.


solderers searches for Companies, Equipment, Machines, Suppliers & Information

convection smt reflow ovens

Component Placement 101 Training Course
Hot selling SMT spare parts and professional SMT machine solutions

Reflow Soldering 101 Training Course
2024 Eptac IPC Certification Training Schedule

Best Reflow Oven
Global manufacturing solutions provider

Training online, at your facility, or at one of our worldwide training centers"
design with ease with Win Source obselete parts and supplies

Low-cost, self-paced, online training on electronics manufacturing fundamentals