No wetting on connector latches

Electronics Forum | Thu Sep 02 05:12:15 EDT 2004 | doi

I am using a triad connector and have problem with wetting at both connector latches.Observed that the leads have very good shiny wetting however concerning the latches the solder just seem to disappear to thin airafter reflow.The connector has a gui

No wetting on connector latches

Electronics Forum | Thu Sep 02 09:51:53 EDT 2004 | davef

We see latches from some suppliers that just are not solderable. Usually the nickel plate on the latch is poor, allowing the nickel to corrode, and requiring a more active flux [if you're lucky]. But lots of times, you end-up with partial wetting,

Print solder paste on test pad on OSP board

Electronics Forum | Tue Sep 14 08:14:07 EDT 2004 | Rob

Hi, There are "Fluxbuster" or "Rotator" pins on the market - we had to use them a few years ago on a flexy board (with OSP). There is some info from one source at the following link: http://www.isiconnectors.com/mfrs/idi/idipr.htm#Rotator We got

Labeling of SMT solder stencils

Electronics Forum | Tue Sep 14 13:40:50 EDT 2004 | paul_boxboro

I feel your pain. Your company may already be using Kapton tape labels for their board serial numbers labels. Kapton is able to withstand repeated wash and heat cycles, and can be printed on a typical Zebra printer. The key to a successful and accura

Evaluating / Qualifying Solder Paste

Electronics Forum | Mon Sep 20 16:27:58 EDT 2004 | blnorman

Besides the processing tests (different print speeds, print delay times, etc.) one test we've had to use is humidity exposure. Solderballing due to high outside humidity is a problem in our plant. So we expose paste to 85% humidity for various time

Coating adhesion problems

Electronics Forum | Mon Sep 20 19:46:16 EDT 2004 | pabloquintana

We use Envibar UV 1244 to coat our PCBs after wave soldering. We clean them with alcohol, and then we coate them manually with a brush. Then they are passed through a UV Oven. We have adhesion problems, and we started by looking at the Envibar, but

Lead free Solder Paste troubles !!!!

Electronics Forum | Tue Sep 28 10:37:45 EDT 2004 | russ

Lets not forget about shipping costs,lead times, and bad lot recovery plan(s)on product rec'd from China. We are paying $.096 per gram (SAC405)with 4kg per wk usage. Shipping is free, stock maintained locally with 2 hr. delivery if necessary. Russ

Lead free Solder Paste troubles !!!!

Electronics Forum | Wed Sep 29 11:02:30 EDT 2004 | habba

Hi all ! I have a very simple ( maybe stupid ) question : Can we mix the lead-free components with 'Pb components' ? I mean, some component would lead-free, but it is only 5% of the whole. Will I have problems on wave and on reflow ? Thanks for hel

Lead free Solder Paste troubles !!!!

Electronics Forum | Fri Oct 01 16:21:15 EDT 2004 | sarah104

I second that one Glenn. I have had really solid support from my paste company. Our guy is Kevin with Aimsolder. He is quick to respond and very knowledgable. We used a cheaper paste a while back, but never ever got any support. I wont make that mist

PBGA overprint

Electronics Forum | Thu Sep 30 17:36:17 EDT 2004 | GIO

i have a 0.5 pitch(19x19 pbga array) ..with a pad of 20 mils (thou) , solder mask is same...(20th..)..and an stenCil aperture of rectangular 22 X 22.1 thou...WHICH SHOWS..I AM HAVING AN OVERPRINT..MY PASTE IS A NO-CLEAN.. COMMENTS PLS...


soldering searches for Companies, Equipment, Machines, Suppliers & Information

Beau Tech
Beau Tech

A US manufacturer of quality hand tools for those engaged in the repair, rework, R & D, testing, and assembly of electronic components and printed circuit boards from Through Hole to 2Mil Pitch Surface Mount.

Manufacturer

98 Elm St.
Portland, ME USA

Phone: 1-207-775-6139