Electronics Forum | Mon May 21 08:51:14 EDT 2012 | fredc
We have been seeing this in the nozzles we have made. We will building all new LED nozzles out of teflon where physically possible. Many of the new Cree LED recomendations are for teflon nozzles. In some that teflon was not recomended teflon was the
Electronics Forum | Tue Oct 16 17:32:04 EDT 2001 | scott
Anybody have any experience with SMT and PTH assembly on Teflon Bare Boards?
Electronics Forum | Mon Oct 08 20:50:37 EDT 2001 | ksfacinelli
What material are you using? There are a great deal of different Teflons (in the family of Teflons) material....is it from Gore or Rodgers???? Does it have aluminum backing?? More information necessary, Kevin
Electronics Forum | Wed Oct 17 18:42:37 EDT 2001 | scott
Any processes that I need to be aware of that differs from standard FR4 during reflow and wave soldering? I've read one of the problems is the thermal expansion of teflon is quite different from copper. I've also seen a "blurb" where teflon absor
Electronics Forum | Mon Oct 08 17:01:19 EDT 2001 | upinder
Hi All. Need some immidiate help. I need to know any / all basic info regarding Teflon PCBs. Any special requirements for assembly on SMT and thru-hole lines, like profiles, placemnt , wave etc. Will there be some basic / big differences in comparis
Electronics Forum | Fri Oct 26 17:01:52 EDT 2001 | davef
We process no Teflon boards. Companies, such as Rogers and Taconic, make laminates of Polytetrafluoroethylene [PTFE] er �Teflon�. Common �Teflon� laminates are: * Woven glass / PTFE * Random microfiber glass / PTFE * Ceramic / PTFE * Woven glass /
Electronics Forum | Tue Oct 16 17:38:42 EDT 2001 | lileubie
Depending on the type of teflon material, thickness, and reflow profile requirements, these will have a direct bearing on your maximum process allowable PCB pallet size. You'll want to be careful on how big the PCB or pallet is. Larger teflon PCBs
Electronics Forum | Tue Oct 16 17:42:56 EDT 2001 | lileubie
What do you need to know? ~ Glenn
Electronics Forum | Thu Apr 25 04:22:14 EDT 2002 | ianchan
We have an internal debate whether to calibrate equipment using K-type thermocouple made out of : 1) fibreglass braided, with a 482 deg-C peak-measurement properties? 2) teflon FEP(fluorinated Ethylene Proplene), with 204 deg-C peak-measurement p
Electronics Forum | Tue Jun 23 19:00:03 EDT 2009 | isd_jwendell
I don't know about removing the teflon insulation, but we weld our thermocouples.