Electronics Forum | Tue Jul 28 07:02:59 EDT 1998 | smd
Right now we are taping the goldfingers which is effective but also expensive. Also, some tape was leaving yellow marks on the goldfingers. We're trying the so-called goldfinger glove from Steven's Products. It's a very small company (probably one gu
Electronics Forum | Mon Aug 03 08:29:24 EDT 1998 | Dave F
SMD: Sounds interesting. What is the contact information on Steve? Dave F | Right now we are taping the goldfingers which is | effective but also expensive. Also, some tape was leaving yellow marks on the goldfingers. We're trying the so-called go
Electronics Forum | Mon Aug 03 08:23:37 EDT 1998 | smd
Stevens Products (supposedly around since 1937) 128 N. Park St. E. Orange, NJ 07019 Tel 973-672-2140 Contact: Ross Stevens, Jr. They'll take a PO but terms are net 30 Right now we are taping the goldfingers which is | effective but also expensive. A
Electronics Forum | Thu Jul 23 22:50:38 EDT 1998 | Steve Gregory
Hey youse guyz... We're finally getting our first real job at the start-up I'm working at. It's actually a pretty unique little board too. Simple as all get out, but unique. You're not gonna believe what this goes into...guess? (I bet ya' you'll neve
Electronics Forum | Wed Jun 17 16:19:10 EDT 1998 | Ryan Jennens
| We are facing a problem of high contamination on boards after wave soldering. We want the contamination to be under 24 ugm/inch square. We are using a no clean flux with the spray fluxer unit of wave soldering. The contamination is higher on the e
Electronics Forum | Mon Jun 08 20:03:07 EDT 1998 | Dave F
| Chiakl | Ion Chromatography has been perfectly described by Dave, but here are a couple of extra considerations: | Ion Chromatography will tell you precisely what is present on the surface of your board/assembly but it will not tell you whether it
Electronics Forum | Fri Jun 05 15:06:26 EDT 1998 | Dave F
| I have just been assigned to look into the ionic chromotograhy test on our PCBA but I have zero knowledge. Could anyone help to explain what is this test about? Is it | a) a destructive test? | b) What is the measurement unit of this test? | c) Wh
Electronics Forum | Fri Jun 05 10:24:56 EDT 1998 | Earl Moon
| I have just been assigned to look into the ionic chromotograhy test on our PCBA but I have zero knowledge. Could anyone help to explain what is this test about? Is it | a) a destructive test? | b) What is the measurement unit of this test? | c) Wh
Electronics Forum | Wed May 27 10:15:52 EDT 1998 | Doug Romm
Just wanted to add a few comments on the discussion of how to identify palladium parts. Generally, there is no "clear-cut" way to identify Pd versus Sn/Pb. It mainly comes with experience. Any part that is is plated prior to being trim/formed will
Electronics Forum | Mon May 18 10:54:46 EDT 1998 | Jerry
If it's really low volume I would only invest in a stencil printer and convection reflow oven to start with. If you want to go really low budget get a manual unit such at one from Transition Automation. Make up some really good shop aids and have s