Alpha tetra bond stencils vs Vigon SC200

Electronics Forum | Sun Apr 05 07:00:31 EDT 2015 | vitrost

After washing a tetra bond stencil at PBT machine (Vigon SC200, 50 deg Celsius by 20 minutes) some signs of glue degradation were seen. Does anybody have an experience washing tetra bond in Vigon? What temperature regime is preferable? Thanks

Stencil Cleaning / Zestron / Vigon

Electronics Forum | Tue Aug 23 10:59:37 EDT 2005 | cyber_wolf

Is there anyone out there using Zestron Vigon SC200 stencil cleaning solution? We were told that it can be used to clean SMT adhesive, water soluble, and no clean paste flux. Can anyone tell me anything about this stuff ?

wave finger cleaner solution

Electronics Forum | Fri Aug 01 09:44:42 EDT 2008 | pjc

Try Zestron Vigon RC 101. This mixes with tap water. Electrovert does not recommend DI water due to its corrosive nature. http://www.zestron.com/fileadmin/zestron/overviews-tis/usa/ti/ti-vigon-rc101-usa.pdf

wave finger cleaner solution

Electronics Forum | Wed Jul 30 09:07:14 EDT 2008 | grics

Zestron's Vigon RC-101...Good with no clean

VIGON A200 and aluminium electrolytic capacitors problem

Electronics Forum | Mon Nov 25 09:45:29 EST 2013 | processman

Are you using zestron corrision inhibiter Ci20 also?

VIGON A200 and aluminium electrolytic capacitors problem

Electronics Forum | Wed Nov 27 06:06:59 EST 2013 | luciano

Thanks!

VIGON A200 and aluminium electrolytic capacitors problem

Electronics Forum | Fri Dec 06 06:02:25 EST 2013 | luciano

Thanks for the advice!

Washing Screens - Foam Everywhere, Help!

Electronics Forum | Tue Nov 01 08:22:37 EDT 2016 | jandon

Maybe you could try Zestron Vigon plus DF 30

Stencil cleaner

Electronics Forum | Tue Jan 23 23:22:18 EST 2007 | jovial_guy23

If you are looking for an effective cleaning performance with long bath life and environmental friendly nature, then definitely VIGON SC200 is a very good choice...You would not regret it...If you want to try out, perhaps you can ask them for VIGON S

raw copper on pcb

Electronics Forum | Thu Jun 07 05:11:42 EDT 2012 | cp38260

Hi, I have pcbs (Duroid/RT 5880) with raw copper, soldered in vapour-phase chamber at 230 degrees Celsius. During soldering, copper gets tarnished. Cleaning with Vigon A250 removes the tarnished layer. Indeed, in the VigonA250 techn. datasheet it is

  1 2 3 4 5 6 7 Next

vigon searches for Companies, Equipment, Machines, Suppliers & Information

Software for SMT

High Throughput Reflow Oven
IPC Training & Certification - Blackfox

Training online, at your facility, or at one of our worldwide training centers"
SMT feeders

High Precision Fluid Dispensers
Electronic Solutions R3

"Heller Korea"