I have a customer who's solder paste is drying out on their ... - Feb 09, 2011 by Steve
Some solder paste formulations can be frozen with no effect.... - Feb 10, 2011 by davef
Going to do that tomorrow. Thanks for the reply. ... - Feb 10, 2011 by Steve