We have a problem with our Unleaded wave solder machine only... - Jun 13, 2012 by Brett
Sorry, but I don't have a quick and easy answer. Before jump... - Jun 13, 2012 by davef
It is possible that there is nickel contamination in the gol... - Jun 13, 2012 by KaHrpr
Yes pads are still gold after the wave soldering process ev... - Jun 14, 2012 by Brett
That you can get good solder flow when hand soldering seems ... - Jun 14, 2012 by davef
Good info above from davef Solder pot contamination seems l... - Jun 15, 2012 by Hegemon
Measured the pot temprature independantly from the software ... - Jun 18, 2012 by Brett
It's possible that if the nickel on your board was skip plat... - Jun 21, 2012 by davef
Are you spray fluxing ? If so, check that you are getting fl... - Jun 22, 2012 by Graham
Spray fluxing yes but have checked the uniformity by using a... - Jun 22, 2012 by Brett