PTH Solder Short | 3 April, 2005

What is the minimum pitch for PTH component not tend to have solder shorts during wave soldering process.

reply »

#33518

PTH Solder Short | 4 April, 2005

It depends on the component and the land, but 0.1 inch is safe.

reply »

jimih280

#33520

PTH Solder Short | 4 April, 2005

that depends on clinch direction, length, and angle. .200" hole center to center is usually safe for all automatic insertion equipment.

reply »


RDR

#33525

PTH Solder Short | 4 April, 2005

Depends on a lot of things as suggested above but we solder land to land spacings of .02" (.5mm) with no shorting.

Russ

reply »


URL

#33529

PTH Solder Short | 4 April, 2005

IPC may help, otherwise there are many factors: Are the PTH clinched or straight? If straight, what length protrusion? What direction are the parts running thru wave? Is product on a pallet?

Not to mention your soldering process: What type of machine are you using? Nitrogen blanket or none? Speed of the conveyor for this product?

Finally your board fab carries a few factor to think about: Type of mask finish. Is there mask between the leads or not? Is this a single sided or double sided product?

A quick fix (if you�re gluing SMT to the bottom first) is to have your stencil cut so a strip of adhesive is between the two leads in that might short. It acts a natural short preventer and cost nothing to implement.

reply »