Good afternoon all, I have been trying to find a solution... - Jun 18, 2010 by Sid
Our best suggestion - get the copper balanced and if possibl... - Jun 24, 2010 by davef
Consider using wavesolder pallets that keep the board flat d... - Jun 25, 2010 by SC
Thanks for you suggestions, guys. davef, I am gonna get w... - Jun 25, 2010 by Sid
Is this a single PCB or a multi-up array? At the very least... - Jun 29, 2010 by dontfeedphils
There are some good suggestions here...reflow pallets, and c... - Jun 29, 2010 by robgd3
Sid, Try baking the boards before running, to insure no m... - Jul 01, 2010 by Julia
Thanks to all for their inputs. @Hexielectronics, I am no... - Jul 01, 2010 by Sid
Try titanium edge stiffners on the PCB before making solder ... - Jul 09, 2010 by Mark