Electronics Forum | Tue Sep 01 10:39:30 EDT 1998 | Mike
| | | We are experiencing shorting on a BGA. The part has a 1mm pitch with a 196 I/O count. The problem seems to pop up without warning & disappear in the same manner. | | | Our pad design is .020" diameter pads with .025" solder resist diameter.
Electronics Forum | Mon Apr 01 20:10:24 EST 2002 | davef
Oh. [Howabout if I smack you?] If ahma connectin� wif whut yer sayin�, you: * Don�t like the appearance of the glue slobberin� out from under the component even though there is no apparent glue on solderable surfaces. * Concerned about the hydrosco