Full Site - : immersion silver shelf life (Page 4 of 14)

Heraeus Electronics Develops New Production Friendly Flexible End Termination Ink

Industry News | 2023-04-03 13:41:12.0

Heraeus Electronics is pleased to announce the development of a production friendly, flexible passive component termination ink. ET2010 Flexible End Termination Ink is a first of its kind material in the market utilizing advanced polymer technology. When compared to current thermoset, epoxy-based inks in the market, Heraeus' solution offers easier shipping, storage, and handling at room temperatures.

Heraeus

Immersion silver life span

Electronics Forum | Wed Apr 13 05:48:52 EDT 2005 | charly

hi' i need advise on immersion silver PCb shelf life. 1) what is the shelf life for Immersion silver PCB? 2) iF PCB expire, can we bake the immersion PCB? what temp & duration? 3) How long can we keep the pCB again after rebaking? (with vacuum seal)

Immersion silver life span

Electronics Forum | Thu Apr 14 06:00:01 EDT 2005 | bryan

The shelf life of immersion silver is 6 to 12 months in good storage conditions. The finish is usually coated with a protective layer that inhibits oxidation (like with copper OSP). Care must be taken when handling the boards as the protective la

immersion Gold life span

Electronics Forum | Mon Jan 08 17:32:47 EST 2007 | Board House

Hi Oswald, Shelf life with ENIG if vacuum sealed and kept in controled enviroment would be 12 to 14 months. Shelf life in shrink wrap - No recomended packaging, 6 moths. If Shelf life goes over the 12 -14 months - Baking ? I would not suggest re-b

immersion Gold life span

Electronics Forum | Mon Jan 08 03:16:12 EST 2007 | oswald5087

hi' i need advise on immersion gold PCb shelf life. 1) what is the issue shelf life or expire for Immersion gold PCB? 2) How long we can keep the PCB? (with vacuum seal and without vacuum seal) 2) iF PCB expire, can we bake the immersion PCB? what t

Immersion silver life span

Electronics Forum | Wed Apr 20 08:06:21 EDT 2005 | davef

We'd reject the boards because: * Vacuum seal is punctured. * HIC is expired. One of the nice things about immersion coatings is that the fab can rework the coating. You cannot do that with other coatings. Finally, every HIC that we investigated c

Immersion silver life span

Electronics Forum | Fri Apr 15 05:52:20 EDT 2005 | charly

hi Jon, does it mean the protective layer is coated after the immersion silver process? if we need to bake the PCb due to moisture issue, then we can not hold the pCB long due to the missing protective layer even with vacuum seal environment

Immersion silver life span

Electronics Forum | Wed Apr 13 07:10:17 EDT 2005 | masters

In addition,how to deal with the misprint immersion Ag PCB?Now,we just remove the paste,clean it,and exposed in air for 2 hours,and then put to use.

Immersion silver life span

Electronics Forum | Mon Apr 18 20:44:30 EDT 2005 | davef

Charly: Why do you "need to bake the PCb due to moisture issue", if you're not going to use the board? Why bake the board, just to put it back in storage, absorb moisture, and require baking again?

Immersion silver life span

Electronics Forum | Wed Apr 20 01:08:16 EDT 2005 | charly

actually, i received a shipment from supplier where the vacuum seal was puntual and the HIC is out of order, the supplier ask me to bake and keep back into the store, but i worry is there any quality impact if i do so?


immersion silver shelf life searches for Companies, Equipment, Machines, Suppliers & Information