Electronics Forum | Thu Mar 29 15:50:35 EST 2001 | tomgervascio
We've think that with seen solder shorts under BGAs after wave soldering the boards. In addition, it seems to be related to a certain soldermask configuration over the topside BGA vias.. THere is one vendor,A, that is applying soldermask after HASL,
Electronics Forum | Wed Oct 06 09:40:49 EDT 1999 | Mark Quealy
I have an adhesive dispenser in my workcenter but I rarely use it. I've replaced this process with wavesolder pallets for bottom side PTH soldering, ocassionally gluing parts left exposed by the pallet. So I was thinking of selling the dispensing equ
Electronics Forum | Fri Aug 10 04:19:05 EDT 2001 | wister
There are lots of voids at solder joint of chips,the thickness of multilayer pcb is 3.2mm,top side have lots of chip component and bottom side has several BGA and QFPs.For top side profile,the preheat time is about 100s,soak time is about 75s,time ov
Electronics Forum | Mon Sep 21 20:45:55 EDT 2009 | davef
10.4. Pre-Cure Examination. Immediately after material application, the uncured conformal coating shall be examined for: a. Bubbles and Air Entrapments. These defects shall be broken by vacuum, with a sharp probe, or other appropriate tools. b. Bridg
Electronics Forum | Mon Jun 14 09:16:58 EDT 1999 | Adam Pratt
| | | | | Hello all! | | | | | Recently we got a problem about the Funtional test. Some boards passed tests by using the auto-fixture(vacuum), but failed by using manual test fixture(need to plug CPU, DIMM etc.). The error symptom is no picture. We d
Electronics Forum | Mon Jun 14 14:30:42 EDT 1999 | Deon Nungaray
| | | | | Hello all! | | | | | Recently we got a problem about the Funtional test. Some boards passed tests by using the auto-fixture(vacuum), but failed by using manual test fixture(need to plug CPU, DIMM etc.). The error symptom is no picture. We d
Electronics Forum | Tue Sep 28 08:27:55 EDT 1999 | Earl Moon
| if anyone has used or has one of these bga rework stations please give me your opinion on them. I am planning on using the sytem for not only rework but also low volume prototype production for hand built 1 or 2 qty pcb's, so ease of use is impor