Electronics Forum | Tue Jun 29 13:52:32 EDT 2004 | microniks
Where to find detailed information on fluxes? No one seems to know the real difference between Rosin fluxes with colophan, Resin fluxes or synthetic Resin fluxes, No Clean, Low Residues, VOC-Free, Halide-Free, Water Washable with alcohol base, Resin-
Electronics Forum | Tue Jun 29 13:56:27 EDT 2004 | Pierre
Where to find detailed information on fluxes? No one seems to know the real difference between Rosin fluxes with colophan, Resin fluxes or synthetic Resin fluxes, No Clean, Low Residues, VOC-Free, Halide-Free, Water Washable with alcohol base, Resin-
Electronics Forum | Mon Jul 18 18:36:01 EDT 2005 | slthomas
"thomas, why isn't it process control," Minute detail, really. Defects aren't a measurement of process parameters, they're the result of them (and a few other things that have been mentioned). SPC measures process parameters. It is preemptive, and
Electronics Forum | Wed May 20 17:56:51 EDT 2009 | dyoungquist
I have attached a pdf showing the dimensions for the QFN we placed. First, The pins on the part are not only on the bottom side but also wrap around to come up each of the 4 sides of the part as shown in the side view in the attached pdf. This i
Electronics Forum | Mon Sep 17 16:03:13 EDT 2001 | jschake
The results from an experiment comparing 27 different combinations of pad dimensions concluded that the pad design with 15 mil pad length, 12 mil pad width, and 9 mil pad separation produced the best assembly yields. A 5 mil thick laser cut stencil
Electronics Forum | Wed May 14 15:15:03 EDT 2008 | boardhouse
Hi Scott, I have worked for a State side PCB Manufacture and now a Taiwan Manufacture. At both shops the up charge was based on how many up the pallet array was plus layer count and complexity of product, charges ranged from free to 15%. Standa
Electronics Forum | Tue May 12 10:03:12 EDT 2009 | daan_terstegge
Hi All, I see more and more components like QFN or LGA with bottom-only terminations,with landpatterns getting finer all the time. I have no ppm-figures of our process, but based on a benchmark study by Agilent I'd say that 500 ppm is a decent value
Electronics Forum | Wed Sep 18 14:12:40 EDT 2013 | pjchonis
Hello Bachman. SAC305 is the most common lead-free solder alloy, not only for wave soldering but also selective. Most of our selective customers (especially automotive) are using SAC305. What is more important than the alloy to consider is the flux
Electronics Forum | Mon Mar 26 16:58:53 EDT 2018 | solderingpro
Is there anything stopping you from replacing the flat belt solution to a continuous running steel roller chain conveyor? - From there (depending upon board temperature) you should be able to buffer your boards in a vertical buffer station if neede
Electronics Forum | Thu Mar 26 13:31:37 EDT 2020 | rgduval