Electronics Forum: conformal coating keep out (Page 1 of 24)

UV cure conformal coating

Electronics Forum | Thu Mar 31 10:14:06 EST 2005 | davef

There's some nice low-VOC uV coatings out there. We don�t use uV cured coatings, but try: * http://www.emersoncuming.com * http://www.dymax.com * http://www.mgchemicals.com * http://www.loctite.com * http://www.humiseal.com Be aware that uV co

conformal coating

Electronics Forum | Wed Jul 06 20:15:51 EDT 2005 | Gary Bremer

The good old days weren't all that bad. When I needed to have a specification callout for a conformal coating on an engineering drawing, I just used MIL-I-46058, type UR (for example), and the drawing checkers were quite happy. Since MIL-I-46058 ha

Is conformal coating necessary?

Electronics Forum | Thu Mar 08 01:19:16 EST 2001 | Mike Moninger

The environment essentially defines the need for coating. "Inside" may mean inside a men's locker room with attendant high humidity or inside a climate-controlled clean environment. Conformal coatings offer protection against moisture, fungus, chemi

Simple conformal coating machine

Electronics Forum | Thu Sep 10 17:13:31 EDT 2015 | tombstonesmt

There are factors that manufacturers have taken into consideration when dealing with coating. On/off times, dispense speeds, heights, etc.. Dedicated software with tools to easily map out paths are a godsend. We made our own coating machine with a s

Problem with conformal coating

Electronics Forum | Sun Apr 10 03:25:35 EDT 2005 | Peter

Normally, some conformal coatings do not have very good wetting properties, that should be basic function of a good coating material (the same reqirement as avoid bubbles during coating process)! For UV curing conformal coatings, you can try Lackwe

Problem with conformal coating

Electronics Forum | Thu Feb 17 15:01:23 EST 2005 | davef

We're not familiar with your DYMAX #984-LVUF. The problem is not with your conformal coating. The problem is with your 0805 [and not all of 0805, probably just those from a specific supplier]. This lack of coverage of components is called dewetting

conformal coating selection

Electronics Forum | Thu Nov 23 23:59:25 EST 2000 | terry sun

Hello to all out there, We're considering CC process,and would like to know some defferences between SSC3 of Electrolube and Humiseal 1B73, yes,I know that SSC3 is silicone one,and Humiseal 1B73 is solvent based acrylic as well as other basic propert

Simple conformal coating machine

Electronics Forum | Fri Sep 11 12:08:10 EDT 2015 | derrikf

I built one using an old Asymtek Automove. When all was said and done, it cost less than $400, including what was paid for the machine itself. It's a very basic setup, (air over syringe), but for our needs it does everything and more. With air to syr

Re: conformal coating after rework

Electronics Forum | Fri Jan 22 14:31:14 EST 1999 | Dave F

| I have boards coated with Humiseal 1B73. At a late point mfg. site we need to remove a series of 0603 resistors for optioning purposes. I have been trying to determine the fastest, easiest way to re-coat the pads after removal. Drying time of the c

Ink marking under conformal coating

Electronics Forum | Mon Jul 02 03:55:07 EDT 2012 | mccabekev

We are having a problem with inspection markings on our boards running when conformal coating is applied We have tried standard permanant markers, and also paint markers, but both run when the coating is applied. There must be someone out there who

  1 2 3 4 5 6 7 8 9 10 Next

conformal coating keep out searches for Companies, Equipment, Machines, Suppliers & Information

Selective Soldering Nozzles

Training online, at your facility, or at one of our worldwide training centers"
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
PCB Handling with CE

Smt Feeder repair service centers in Europe, North, South America
PCB Depanelizers

"Find out how you can receive priority in SMTnet Search with out Sponsor membership."