Electronics Forum: pads of pcb oxidation (Page 1 of 16)

Non wetting spots of flex PCB pads

Electronics Forum | Thu Jun 29 04:50:42 EDT 2023 | SMTA-70263692

This looks like it could be related to oxidation.Do you per-bake your pcb before assembly to remove any moisture inside your board panel?

Non wetting spots of flex PCB pads

Electronics Forum | Thu Jun 29 10:53:30 EDT 2023 | matouschekd

Repairing these PCBs was not an option due to the delivery amount. Oxidation is unlikely, as these anomalies were visible right after unpacking them and the humidity card was not suspicious. We have since decided not to use these PCBs as the risks w

Inspection of pads in PCB

Electronics Forum | Tue Dec 05 22:27:05 EST 2023 | padawanlinuxero

Hello, I am experiencing issues with one of my PCB suppliers. Specifically, I am having trouble with solder shorts occurring on a SOIC8 component, and always in the same pads. Upon inspection with a microscope, I discovered that three of the pads ar

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 13:55:05 EDT 2014 | horchak

Ok lets put it this way. If the PCB house used a high quality mask and properly applied it to a properly cleaned surface and properly cured it, then as Dave stated above there are only two things that can destroy it. Excessive heat and overly aggress

Non wetting spots of flex PCB pads

Electronics Forum | Thu Jun 29 09:55:54 EDT 2023 | matouschekd

Yes, i tried cleaning it with PCB-Cleaner. Sadly, no success

Non wetting spots of flex PCB pads

Electronics Forum | Fri May 12 19:42:05 EDT 2023 | emeto

Have you tried cleaning these spots with anything?

Non wetting spots of flex PCB pads

Electronics Forum | Fri May 12 08:58:04 EDT 2023 | tommy_magyar

This is a defect in all IPC classes. Solder has not wetted to the land where solder is required.

Automated attachment of wire to SMT pads

Electronics Forum | Wed Jul 17 10:44:19 EDT 2013 | gregcr

Hi All, Has anyone seen or used equipment that is capable of automating the process of attaching hookup wire directly to a large SMT pad? Soldering, ultrasonic? I'm looking to see if there is a machine that is capable of automatically taking a tef

Non wetting spots of flex PCB pads

Electronics Forum | Fri May 26 04:58:19 EDT 2023 | auriga2001

I agree with the two other replies. Left alone, it is a defect. If it's just excess adhesive or coating, you can use IPC-7711/7721 'Rework, Modification and Repair of Electronic Assemblies' for guidance on removing. Section 2.3.1 explains how to te

Floor life pcb assembly

Electronics Forum | Wed Apr 23 19:00:39 EDT 2008 | stevek

It depends on the laminate but a PWB is like any other MSL component. Some fab shops are only waranting standard FR4 laminates for 45-60 days when processed at lead free temperatures. The best thing I can say is to try some weight gain/loss experim

  1 2 3 4 5 6 7 8 9 10 Next

pads of pcb oxidation searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830

used smt parts china

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
Win Source Online Electronic parts

Training online, at your facility, or at one of our worldwide training centers"
SMT feeders

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
PCB Handling Machine with CE

Component Placement 101 Training Course
PCB Handling with CE

Software for SMT placement & AOI - Free Download.
SMT spare parts

Thermal Transfer Materials.