Re: Residue/Cure Testing Of Solder Mask

Electronics Forum | Fri May 29 17:48:34 EDT 1998 | Earl Moon

| | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not localize

Re: Residue/Cure Testing Of Solder Mask

Electronics Forum | Sat May 30 08:24:09 EDT 1998 | Dave F

| | | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not locali

Re: Residue/Cure Testing Of Solder Mask

Electronics Forum | Sat May 30 12:51:29 EDT 1998 | Earl Moon

| | | | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not loca

Re: When using noclean flux or clean flux process?

Electronics Forum | Wed Sep 22 02:45:23 EDT 1999 | Brian

| | Dear All, | | | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | | | I mean that I wonder

Re: Residue

Electronics Forum | Wed May 27 09:56:39 EDT 1998 | Chrys

| | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not localize

Re: Residue/Measuring Flux

Electronics Forum | Wed May 27 15:09:30 EDT 1998 | Dave F

| | | | We recently made the switch to no-clean and the wurface mount is turning out beautifully. However, the wave solder process continues to put up a fight; we are getting a white residue on the surface of the PCB. The residue is not locali

Re: Solderability on Immersion Gold

Electronics Forum | Thu Mar 02 21:24:27 EST 2000 | Dave F

Glen: As I mention in an earlier response in this thread, I think someone at Steve's plant (or may be in his packaging spec for the fabs) is doing something to leave a residue, but I'm also thinking solder mask ... ENIG can be applied before or aft

Re: Clean before conformal coating?

Electronics Forum | Fri Jan 05 09:23:10 EST 2001 | Brian Toleno

While there may not be any specific requirement to cleaning prior to coating, cleaning an assembly prior to coating will only serve to increase the reliability and integrity of the coating. Some residues from low-solids fluxes can interact with conf

Re: Clean before conformal coating?

Electronics Forum | Sat Jan 06 22:09:53 EST 2001 | Greenman

Cory, I've got a lot of experience of testing of this type. The physical (not chemical) nature of the flux residues is the crucial issue in compatibility. If you have a softer residue (either caused by a thick initial solder paste deposit, or a low p

Re: baked on water soluble flux residue betwwen fine pitch comp.

Electronics Forum | Fri Dec 01 16:02:33 EST 2000 | Jim M

Thanks for your reply. I 've tried to clarify and answer your questions. The water soluble paste used is WS3060, type 4. The boards are sent through a inline di cleaner after reflow. There is a hot Di waterwash, rinse and then hot air to dry the wa


residues searches for Companies, Equipment, Machines, Suppliers & Information

One stop service for all SMT and PCB needs

Training online, at your facility, or at one of our worldwide training centers"
Sell Your Used SMT & Test Equipment

High Resolution Fast Speed Industrial Cameras.
SMT feeders

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
2024 Eptac IPC Certification Training Schedule

Software for SMT placement & AOI - Free Download.
Fully Automatic BGA Rework Station

"Find out how you can receive priority in SMTnet Search with out Sponsor membership."