Electronics Forum: wash bake (Page 2 of 15)

Baking assemblies after ultrasonic water wash

Electronics Forum | Wed Jun 24 05:08:37 EDT 2009 | Mark

Try immersing the assembly in IPA for 30 minutes. IPA is hydroscopic ans will drive off most of the water. Dry the assembly. Then bake at 110°C for 2 hours.

Baking assemblies after ultrasonic water wash

Electronics Forum | Wed Jun 10 22:47:17 EDT 2009 | davef

You're correct that JEDEC J-STD-033 defines baking condidtions for moisture sensitive components. Why do you want to bake assemblies after cleaning? Search the fine SMTnet Archives for threads like: http://www.smtnet.com/forums/Index.cfm?CFApp=1&Me

If we could bake the Board with OSP finish?

Electronics Forum | Fri Aug 06 10:07:50 EDT 2004 | blnorman

OSP has limited elevated temperature exposure capability. Couple that with the fact that solvents (IPA in particular) will remove the OSP. The more material you loose the higher the chances for pad oxidation. We ran an experiment with board washin

Baking assemblies after ultrasonic water wash

Electronics Forum | Thu Jun 25 20:01:54 EDT 2009 | davef

Shanelo Technologies Given that isopropyl alcohol [IPA] is produced by combining water and propene. How does soaking a board in water and a flammable liquid drive off water?

Baking assemblies after ultrasonic water wash

Electronics Forum | Wed Jul 01 05:26:31 EDT 2009 | kpm135

But the boards and parts on the boards are also hygroscopic(no not a typo I did a search on hydroscopic and it is not a word the actual word is hygroscopic look it up if you don't believe me) so if you have two hygroscopic materials which one wins?

Baking assemblies after ultrasonic water wash

Electronics Forum | Tue Jun 09 18:44:20 EDT 2009 | dyoungquist

We are using a water soluble flux which requires the assemblies to be cleaned in an ultra sonic cleaner after assembly. Is there a standard that specifies how long the assemblies need to be baked/dried after being submersed in a water solution for a

Baking assemblies after ultrasonic water wash

Electronics Forum | Thu Jun 11 10:02:36 EDT 2009 | dyoungquist

Our cleaning process involves the assemblies being completely immersed in the water bath of the ultrasonic cleaner. The assembly has a QFP44 on it. Customer stated that when these assemblies have been cleaned with water in the past (at a different

second side reflow of MSD parts after wash

Electronics Forum | Thu Mar 25 09:27:08 EDT 2010 | stepheniii

Thanks I guess I got used to google where the "and" is implied. I searched various combinations and all I could find were threads regarding the pcb's not the components. Does anyone bake their boards after wash before second reflow because of MSD c

second side reflow of MSD parts after wash

Electronics Forum | Wed Mar 24 16:54:38 EDT 2010 | stepheniii

J-STD-033B.1 Says "For cavity packages in which water may be entrpped, water clean processes after first reflow can be an additional source of moisture. This may present an additional risk, which should be evaluated." And it talks about derating if

Do you need to bake after parts are in the Dry Cabinet

Electronics Forum | Mon Jan 30 16:30:55 EST 2006 | GS

Hi James, it could be the problem is due to residual of cleaner media entrapped under low gap of QFP 208 and 0,5 mm lead pitch. I remember in the past we had random problems of failure at test after board wash off process (DI Water wash). We met


wash bake searches for Companies, Equipment, Machines, Suppliers & Information

2024 Eptac IPC Certification Training Schedule

World's Best Reflow Oven Customizable for Unique Applications
Selective Soldering Nozzles

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
Win Source Online Electronic parts

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
PCB Handling Machine with CE

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.


"Find out how you can receive priority in SMTnet Search with out Sponsor membership."