Electronics Forum: wetting (Page 134 of 182)

Wet or Dry Wipe

Electronics Forum | Fri Jan 06 10:49:03 EST 2006 | PWH

We had a bad situation with solvent wipe. One of the solvent supply lines cracked and the solvent got on a cluster of air lines. The air line material reacted poorly and we blew what seemed like one airline per day for a couple weeks. I had to cut

Solder Paste Evaluation

Electronics Forum | Thu Feb 02 09:06:53 EST 2006 | drewake

Sorry, I am jumping into this late - I'm a new user. Our company is looking to perform an evaluation for a new paste. We are looking at a 63/37 no clean - type 3 or 4. Our technology is currently at 0201s, .4mm pitch ICs & .5mm uBGAs. I have

CP6 Maintenance

Electronics Forum | Thu Mar 30 12:38:14 EST 2006 | Tech

Also why I am at it. In the book CP-6 Series Maintenance Manul ( Fuji Part # MNT-C060-11.3E ) in Chapter 4 page 4-1-11 it says " The clutches should therfore be cleaned regularly, using the grease cleaner (ThreeBond 2706) provided with the machine."

Running with sn100c in my solder pot!

Electronics Forum | Tue Jun 27 08:38:03 EDT 2006 | cuculi54986@yahoo.com

I tried some SN100C from AIM... On only one array. It flowed well on the chips but did not like the finish on the SOT23's on the board. I did not have enough arrays to mess around, so we switched it over to SAC305 and had no issues. I'm guessing w

Problems with SN100C in a Soltec Delta C Wave

Electronics Forum | Mon Jun 12 09:08:17 EDT 2006 | Chunks

Hi Grant, Boy, how do I say this - I might have to agree with Wave Master Larry. (Yeah, yeah - I know; Davef and Dr. Shocker will "burn me" again) "We" also solder large thru-hole connectors on with a selective solder machine. They measure 4 by 8

Oop's Pb BGA's in a RoHS process?

Electronics Forum | Wed Jun 21 13:25:16 EDT 2006 | muse95

I see what you're saying - I'm not a process guru by any means. I was going on the premise that SAC melts at a higher temperature than SnPb. Basically I think of it as a BGA is joining solder to solder, unlike an SOIC where it is tinned metal lead t

and you think youve got it hard

Electronics Forum | Wed Jul 12 23:29:23 EDT 2006 | KEN

Ah yes Mechanical Engineers. My previous company hired one Fresh out of College. Ink was still wet on his B.S. degree when he entered the shop. I passed by his desk. He had a CAD drawing on the monitor which he was feverously working on. It showe

Lead Free boards

Electronics Forum | Mon Aug 28 12:44:23 EDT 2006 | actech

WE have been running a leaded product for a few years and while the product is exempt from PB free regulations the components have been comming in lead free reciently and this caused little or no change in the process and or product, However! the Boa

Fibers In Solder Joints

Electronics Forum | Wed Sep 06 11:34:15 EDT 2006 | slthomas

I don't remember ever having that problem with my EKRAs, but you might look at how much fluid you're dispensing on to the cleaning medium if this is occurring while you're using wet cleaning cycles. It could be getting saturated to the point of weakn

Surface Tension vs Part Mass

Electronics Forum | Tue Sep 12 10:55:29 EDT 2006 | slthomas

I found this searching the archives. Unfortunately Bob doesn't seem to have an active site anymore, just references by people he works for. It's a shame, because there was a load of good stuff there. Haven't looked at Phil's site for a while but it's


wetting searches for Companies, Equipment, Machines, Suppliers & Information

SMT feeders

Benchtop Fluid Dispenser
Blackfox IPC Training & Certification

Reflow Soldering 101 Training Course
pressure curing ovens

Software for SMT placement & AOI - Free Download.
Hot selling SMT spare parts and professional SMT machine solutions

Training online, at your facility, or at one of our worldwide training centers"
PCB Depanelizers

Low-cost, self-paced, online training on electronics manufacturing fundamentals