Technical Library: pcbrm and 12 and (Page 5 of 7)

Packaging Technology and Design Challenge for Fine Pitch Micro-Bump Cu-Pillar and BOT (Direct Bond on Substrate-Trace) Using TCNCP

Technical Library | 2015-12-02 18:32:50.0

(Thermal Compression with Non-Conductive Paste Underfill) Method.The companies writing this paper have jointly developed Copper (Cu) Pillar micro-bump and TCNCP(Thermal Compression with Non-Conductive Paste) technology over the last two+ years. The Cu Pillar micro-bump and TCNCP is one of the platform technologies, which is essentially required for 2.5D/3D chip stacking as well as cost effective SFF (small form factor) package enablement.Although the baseline packaging process methodology for a normal pad pitch (i.e. inline 50μm) within smaller chip size (i.e. 100 mm2) has been established and are in use for HVM production, there are several challenges to be addressed for further development for commercialization of finer bump pitch with larger die (i.e. ≤50μm tri-tier bond pad with the die larger than 400mm2).This paper will address the key challenges of each field, such as the Cu trace design on a substrate for robust micro-joint reliability, TCNCP technology, and substrate technology (i.e. structure, surface finish). Technical recommendations based on the lessons learned from a series of process experimentation will be provided, as well. Finally, this technology has been used for the successful launching of the company FPGA products with SFF packaging technology.

Altera Corporation

Effect of Surface Oxide on the Melting Behavior of Lead-Free Solder Nanowires and Nanorods

Technical Library | 2013-07-18 12:12:40.0

Lead-free nanosolders have shown promise in nanowire and nanoelectronics assembly. Among various important parameters, melting is the most fundamental property affecting the assembly process. Here we report that the melting behavior of tin and tin/silver nanowires and nanorods can be significantly affected by the surface oxide of nanosolders.

Department of Chemical Engineering, University of Massachusetts

Difference between Neutral and Acid Salt Spray Corrosion Test

Technical Library | 2019-12-13 00:39:29.0

Salt spray corrosion chamber can test the ability of material and its protective layer to resist salt mist corrosion, or compare the process quality of similar protective layers, at the same time; this equipment is suitable for parts, electronic components, protective layer of metal material and other industrial products. Salt spray test is divided into neutral and acid test. What is the difference between neutral and acid in salt spray test? First, the temperature applied in the test method is different: Neutral test: a. Laboratory:35°C ±1°C, b. Saturated air drums:47°C ±1°C Acid test: a. Laboratory:50°C ±1°C, b. Saturated air drums:63°C ±1°C Second, the production material is different,neutral test chamber adoptes the traditional PVC plates, acid test chamber asopts PP sheet,which is more high temperature resistance and suits strong acid test. Third. Different test methods satisfied Neutral salt spray chamber according to GB/T 2423.17-2008, GB/T 2423.18-2000, salt spray test method and GB/T 10125-1997, GB/T 10587-2006, GB10593.2-1990, GB/T 1765-1979, GB/T 1771-2007, GB/T 12967.388, GB/T 1705.8-2008, etc. In addition to the test methods specified in the national standard, acid salt spray chamber also needs to expand the standard setting such as IEC,MIL,DIN,ASTM,IS,CNS. Last, Comparison of neutral test solutions China: NaCI distilled water solution NaCI mass concentration (50 ±5) g ≤ l pH value 6.5 ≤ 7.2 United States: distilled water solution NaCI mass concentration 5% ±1% pH value 6.5 ≤ 7.2 Germany: NaCI distilled water solution NaCI mass concentration (50 ±5) g ≤ l pH value 6.5 ≤ 7.2 Japan: NaCI distilled water solution NaCI mass concentration 5% ±1% pH pH value 6.5 ~ 7.2 France: NaCI distilled water solution NaCI mass concentration 5% pH 6.5 ≤ 7.2 https://climatechambers.com/articles&latestnews/difference-between-neutral-and-acid-salt-spray-corrosion-test.html

Symor Instrument Equipment Co.,Ltd

Organic Flip Chip Packages for Use in Military and Aerospace Applications

Technical Library | 2006-11-14 12:48:31.0

Content: 1. Bridge from Commercial Reliability 2. Existing PBGA use in Aerospace & Military 3. Drivers: Plastic versus Ceramic Package Weight 4. Attributes of PTFE and Thin Core FC Packages 5. Flip Chip Package Reliability 6. Flip Chip Package

i3 Electronics

SnCu Based Alloy Design for Lower Copper Dissolution and Better Process Control

Technical Library | 2009-02-13 12:29:39.0

To meet the market demand for a best-in-class, low-cost leadfree alloy for wave, selective and dip soldering

Kester

Bridging at Reflow, What is the Cause and Can it be Eliminated?

Technical Library | 2012-04-12 21:25:13.0

Surface mount technology (SMT) started in the 1960s and became more common in the 1980s. It is the dominant technology in use today. Through-hole technology is still in use, and will be for the foreseeable future, but the drive towards miniaturization of

FCT ASSEMBLY, INC.

Using Simulation to Optimize Microvia Placement and Materials to Avoid Failure During Reflow

Technical Library | 2021-12-21 23:11:50.0

This paper cover the following points: - Objective 01: Preprocessing, - Introduction, - Objective 02: Automated FE Scripting, - Objective 03: Postprocessing, Reliability Analysis of PTHs, - Objective 03: Postprocessing, Manufacturability of Microvias

CALCE Center for Advanced Life Cycle Engineering

Issues and Challenges of Testing Modern Low Voltage Devices with Conventional In-Circuit Testers

Technical Library | 2012-12-14 14:25:37.0

The popularity of low voltage technologies has grown significantly over the last decade as semiconductor device manufacturers have moved to satisfy market demands for more powerful products, smaller packaging, and longer battery life. By shrinking the size of the features they etch into semiconductor dice, IC manufacturers achieve lower costs, while improving speed and building in more functionality. However, this move toward smaller features has lead to lower breakdown voltages and increased opportunities for component overstress and false failures during in-circuit test.

Teradyne

Characterization, Prevention and Removal of Particulate Matter on Printed Circuit Boards

Technical Library | 2016-12-22 16:44:04.0

Particulate matter contamination is known to become wet and therefore ionically conductive and corrosive if the humidity in the environment rises above the deliquescence relative humidity (DRH) of the particulate matter. In wet condition, particulate matter can electrically bridge closely spaced features on printed circuit boards (PCBs), leading to their electrical failure. (...) The objective of this paper is to develop and describe a practical, routine means of measuring the DRH of minute quantities of particulate matter (1 mg or less) found on PCBs.

IBM Corporation

Article Design and Experiment of a Solder Paste Jetting System Driven by a Piezoelectric Stack

Technical Library | 2017-12-27 22:52:43.0

To compensate for the insufficiency and instability of solder paste dispensing and printing that are used in the SMT production process, a noncontact solder paste jetting system driven by a piezoelectric stack based on the principle of the nozzle-needle-system is introduced in this paper, in which a miniscule gap exists between the nozzle and needle during the jetting process.

Jilin University