Copper Wire Bond Failure Mechanisms.

Technical Library | 2014-07-24 16:26:34.0

Wire bonding a die to a package has traditionally been performed using either aluminum or gold wire. Gold wire provides the ability to use a ball and stitch process. This technique provides more control over loop height and bond placement. The drawback has been the increasing cost of the gold wire. Lower cost Al wire has been used for wedge-wedge bonds but these are not as versatile for complex package assembly. The use of copper wire for ball-stitch bonding has been proposed and recently implemented in high volume to solve the cost issues with gold. As one would expect, bonding with copper is not as forgiving as with gold mainly due to oxide growth and hardness differences. This paper will examine the common failure mechanisms that one might experience when implementing this new technology.

DfR Solutions (acquired by ANSYS Inc)

Eliminating Ni Corrosion in ENIG/ENEPIG Using Reduction-Assisted Immersion Gold in Place of Standard Immersion Gold

Technical Library | 2023-01-10 20:08:36.0

Nickel corrosion in ENIG and ENEPIG is occasionally reported; when encountered at assembly it manifests as soldering failures in ENIG and wire bond lifts in ENEPIG. Although not common, it can be highly disruptive, resulting in missed deliver schedules, supply chain disruption, failure analysis investigations, and liability - all very costly.

Uyemura International Corporation

Challenges on ENEPIG Finished PCBs: Gold Ball Bonding and Pad Metal Lift

Technical Library | 2017-09-07 13:56:11.0

As a surface finish for PCBs, Electroless Nickel/Electroless Palladium/Immersion Gold (ENEPIG) was selected over Electroless Nickel/Immersion Gold (ENIG) for CMOS image sensor applications with both surface mount technology (SMT) and gold ball bonding processes in mind based on the research available on-line. Challenges in the wire bonding process on ENEPIG with regards to bondability and other plating related issues are summarized.

Teledyne DALSA

Wire Bonding and Soldering on Enepig and Enep Surface Finishes with Pure Pd-Layers

Technical Library | 2012-10-11 19:50:09.0

First published in the 2012 IPC APEX EXPO technical conference proceedings. This paper shows the benefits by using a pure palladium Layer in the ENEPIG (Electroless Nickel, Electroless Palladium, Immersion Gold) and ENEP (Electroless Nickel, Electroless P

Atotech

Gold Wire Bonding Performance and Reliability of ENEPIG Surface Finishes.

Technical Library | 2011-03-30 21:14:33.0

The expression "multifunctional PCB", as a synonym for a PCB which is applicable with a variety of assembly techniques, is already established on the market. That means the PCB can be used for multiple reflow soldering and multiple assembly techniques lik

Atotech

  1  

wedge bond enepig searches for Companies, Equipment, Machines, Suppliers & Information