Technical Library | 2019-05-30 10:59:13.0
In the current economic environment, the ability to reuse ball grid array(BGA) components that have failed due to solder defects may be an efficient way for electronics manufacturers to reduce costs. Cost may not be the only driving factor in the decision to engage in this recycling practice. The increasing demands placed upon the complexity of microprocessors and integrated circuits (ICs) has decreased the availability of some components, and increased their lead time. Because of this, reballing may provide a means to meet schedule, reduce rework turn-around time, and give a manufacturer a decisive advantage over other companies in an ever increasingly competitive market. This article will discuss the process of reballing BGA components (Figure 1), examining preparation (the preform method, the screen method), and cleaning and bake-out.
Technical Library | 2009-11-05 11:17:32.0
Head-in-pillow (HiP), also known as ball-and-socket, is a solder joint defect where the solder paste deposit wets the pad, but does not fully wet the ball. This results in a solder joint with enough of a connection to have electrical integrity, but lacking sufficient mechanical strength. Due to the lack of solder joint strength, these components may fail with very little mechanical or thermal stress. This potentially costly defect is not usually detected in functional testing, and only shows up as a failure in the field after the assembly has been exposed to some physical or thermal stress.
1 |