SOLDERITE ULF-210RN, ULF-210RNI, ULF-250, ULF-300VZ-3, and ULF-500VS are ultra low residue type flux and these are developed for soldering printed circuit board mounted chip componenets and flat ICs which are for miniaturize and high density purpose.
New Equipment | Solder Materials
Alpha has a range of flux cored solder wires for component attach, rework and touch-up soldering for through-hole and surface mount technologies. The range includes no-clean, water-soluble and activated rosin fluxes in a variety of solder alloys. A
Electronics Forum | Sat Aug 28 19:31:36 EDT 2004 | ryufoong
Currently, in my working factory, we facing the flux residue remain on connector after washing. (of course, this is clean process with WS solder paste). So, are there any ways to clean the flux residue rather than go back to wash again? Because wash
Electronics Forum | Sun Aug 29 19:17:34 EDT 2004 | aqueous
Chen, It is always best to place one�s effort on determining the cause and content of the residue rather than trying to work around it. The first thing you must determine is the nature of the residue. Is it flux? In many instances, the residue is
Industry News | 2024-03-18 12:30:34.0
Count On Tools, Inc. (COT), a leading provider of precision components and SMT spare parts, will exhibit in Booth #1332 at the 2024 IPC APEX EXPO, scheduled to take place April 9-11, 2024 at the Anaheim Convention Center in Calif. The COT team will focus on its core product lines at the show:
Industry News | 2011-09-06 15:20:36.0
SMTA China announced the Best Paper/Presentation and Best Exhibit Awards at its annual awards presentation held in conjunction with SMTA China and Hong Kong Chapter Breakfast Reception, which took place August 31, 2011 at the Ritz-Carlton Hotel in Shenzhen.
Technical Library | 2013-04-11 15:43:17.0
With the explosion of growth in handheld electronics devices, manufacturers have been forced to look for ways to reinforce their assemblies against the inevitable bumps and drops that their products experience in the field. One method of reinforcement has been the utilization of underfills to "glue" certain SMDs to the PCB. Bumped SMDs attached to the PCB with a no-clean soldering process offer the unavoidable scenario of the underfill coming in contact with a flux residue. This may or may not create a reliability issue... First published in the 2012 IPC APEX EXPO technical conference proceedings
Technical Library | 2018-11-20 21:33:57.0
There are several industry-accepted methods for determining the reliability of flux residues after assembly. The recommended methods of test sample preparation do not always closely mimic the thermal cycle experienced by an assembly. Therefore, extraction from actual assemblies has become a popular method of process control to assess consistency of post-reflow cleanliness. Every method of post-reflow flux residue characterization will depend on the reflow process followed to prepare the coupon.This investigation will focus on the effect of thermal conditions on the remainder of active ingredients in flux residues after assembly with no-clean solder pastes.
Flux spray coating on a PCB with uniformal thickness down to 5 microns, with clear edge definition and minimal overspray. Can coat large or shoot dots with the same jet.
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/select/technologies-or-options/drop-jet-fluxing
FluxJet Precision Drop-Jet Dispenser - English FluxJet Precision Drop-Jet Dispenser Enables No-Clean Processing and Minimizes Flux Residues Features and Benefits - Precise on-demand drop-jet
Imagineering, Inc. | https://www.pcbnet.com/blog/identifying-and-correcting-solder-bridge-defects/
: No solder mask is present between adjacent pads Spacing of pads is too close Residue accumulation on the surface of a printed circuit board or stencil Misalignment during solder paste printing or