Plating for aluminum wire bonding

Electronics Forum | Tue May 13 21:08:24 EDT 2003 | ramanandkini

Dear Sir, Sorry for the delay in reply. This is regarding MIL standard for bond pull strength: MIL-STD-883C dt.25/08/83 Bond strength (destructive bond pull test); refer table-1 Minimum bond strengths for various wire composition & diameter given.

solder strength

Electronics Forum | Fri Sep 02 09:02:10 EDT 2005 | dougs

you tell me, the customer has started to pull at some of the leads of some IC's with tweezers while de-bugging boards that had failed in the field, he was able to pull some of the leads away from the solder joints, we feel he may be over-doing it a

Plating for aluminum wire bonding

Electronics Forum | Mon Mar 17 10:36:04 EST 2003 | davef

Ramanandkini 14 gm versus 5 gm: 14 gm [even 10 gm] sounds better than 5 gm. We get good bond pull XBAR (high teens) and low sigma (

Plating for aluminum wire bonding

Electronics Forum | Sat Mar 15 20:24:13 EST 2003 | ramanandkini

Thanks Mr.Dave. Sorry for the delay. One of our major prolems in ENIG plated surface is that wire does not stick. For many years we were getting a bond strength of 14 grams in both ENIG and electroplated surfaces. Now one vendor supplies ENIG boards

Solder joint strength

Electronics Forum | Tue Mar 29 14:45:12 EST 2005 | davef

IPC-TM-650 TEST METHODS MANUAL Number 2.4.21.1 Subject: Bond Strength, Surface Mount Lands Perpendicular Pull Method 1 Scope This test method is used to determine the bond strength (breakaway strength) of surface mount lands from substrate materials

how to measure Adhesive strength

Electronics Forum | Tue May 12 07:26:16 EDT 2009 | emmanueldavid

Jorge, The basic thumb rule to measure Adhesive Strength remains as bonded Chips at Post Reflow should not move around or misplace when Your Thumb Finger try to do so which called as Thumb Force Test. However as Dave stated, there are various Stre

Au Wire bonding failure

Electronics Forum | Wed Dec 14 20:17:48 EST 2016 | davef

As I understand, you are wire bond gold wire to gold pad, where the substrate has good bond strength, but the die does not. If bond quality is good, and then drops off rapidly, then it's probably something to do with contamination within the system

COB Issue's (Non-Sticking)

Electronics Forum | Wed May 18 07:22:06 EDT 2005 | davef

Wire bonds don't stick when bonded * Check pull and shear strength. * Depending on point of failure, review parameters. * Listen during bonding, if there is a high pitch buzz, there is vibration in the system somewhere, "seek and destroy". * Get the

Aluminum wire bonding on ENEPIG plated PCB

Electronics Forum | Mon Sep 09 15:38:02 EDT 2013 | arendonk

Hi, We are having issues aluminum wirebonding on ENEPIG plated PCB by a too low pull force and or having lifts (1% range). Could any body advice how to solve this problem? Is there a special wire bond grade required? How to best clean contaminant

Wirebond issues near SM

Electronics Forum | Thu Oct 29 20:19:43 EDT 2009 | 89jeong

Hi. We are doing Au bonding on Al bond pad not Au plated. If pull strength is less than 2.0g, i think that the ball or stich may be lifted from bond pad. And the value become lower after several reflow. I expect that the surface of bond pad may be c