Anyone know what Solder lead use to connect Thermocouple wire to PCB?

Electronics Forum | Wed Jan 21 12:25:45 EST 2015 | dyoungquist

Kester makes a thermocouple solder: Alloy SN10PB88AG2 Flux "44" Core 58 Diam 0.031" I have used this to solder thermocouples to pcbs when profiling for lead-free temperatures. When done you can unsolder the thermocouple and reuse it again. This g

Flux thinning

Electronics Forum | Mon Feb 16 16:52:51 EST 2015 | joe98375

Hello, We are buying a Vitronics-Soltec wave solder machine with a spray fluxer to replace our old Econopak that has a foam fluxer. Currently we thin our flux (Kester 951) in the foam fluxer per Kester PS-20 and PS-22 test kits with kester 110 thinn

Flux thinning

Electronics Forum | Tue Feb 17 10:27:39 EST 2015 | joe98375

Thanks for the info I will definitely be getting a hold of kester.

Air Moisture in Production

Electronics Forum | Wed Dec 08 11:26:04 EST 2010 | davef

3 Printer Area Conditions * As stated earlier, heat and humidity are damaging to solder paste. Ideally, the printing area should be maintained at 40% - 50% relative humidity and 72°- 80°F (22-26°C). In addition, no air (cool or warm) should blow dire

Lead Free paste

Electronics Forum | Tue Nov 07 15:08:59 EST 2006 | russ

here are my thoughts on kester, I have rec'd a sample to qualify here and we cannot even get it out of the cartridge it is so dryed out. Rep informed me that Kester has a problem with its chemistry right now. Product is Mfgr'd in off shore location

AIM, KESTER, OR INDIUM PASTE PREFERRED?

Electronics Forum | Fri Oct 28 14:28:20 EDT 2005 | aespino

Have any of you used or evaluated lead free water soluble paste from kester or indium?

Insufficient Wetting to Lands

Electronics Forum | Thu Nov 21 05:44:07 EST 2002 | kcorrin

We produce several boards with reflowed components on top and bottom. We are finding the solder has wetted to the leads but did not flow completely to the end of the lands. Several factors/causes?: 1) Board warping but paste deposits look good. 2) Mo

Flux not foaming

Electronics Forum | Tue Sep 20 11:28:20 EDT 2011 | russw

We've got a Novastar 12S wave solder machine and we've been using Kester 951 flux for years with no problems. We just got a new bottle of 951 and it does not foam correctly (thin foam with lots of large bubbles). After a lot of back and forth with

AIM, KESTER, OR INDIUM PASTE PREFERRED?

Electronics Forum | Wed Nov 09 12:19:55 EST 2005 | bhu

We have used the Indium sac305 lead free with good results.

BGA non wetting

Electronics Forum | Wed Sep 15 03:04:13 EDT 2010 | genesan

kester 562 clean process and this leaded part.