QFP soldering issue

Electronics Forum | Thu Jan 15 08:39:26 EST 2004 | Patrick

Thanks for the reply, I do know that the HASL finish is "domed " on opposite sides of a QFP site & "smooth" on the other two sides. (ie. Sides 1 & 3 are domed, & sides 2 & 4 are smooth ) depending on the direction the PCB was extracted from sol

Poor HASL Finish known to cause solder shorts?

Electronics Forum | Fri Sep 24 09:49:53 EDT 1999 | C.K.

Hi Folks: We've been having bridging problems on our fine-pitch QFP's, despite thorough inspection of paste height, volume, and placement accuracies....profiles look good also. The bridging is happening after coming out of reflow...one last thing t

Looking for expert opinions, Solderability

Electronics Forum | Fri Jul 23 06:48:23 EDT 2004 | mattkehoe

I am actually getting opinions that point to contaminated copper under the HASL finish. We've seen some "fish eyes" where the HASL is pulled away from the copper exposing a pin hole of copper that can be seen through the HASL finsh. We are planning o

Sn100C HASL Finish on PCB

Electronics Forum | Wed Jan 26 17:36:22 EST 2011 | ck_the_flip

had a quick question regarding compatibility of Sn100C HASL finish and regular Sn63 solder paste. Does the thermal profile have to reach Sn100C eutectic temps. in order for the Sn 100C HASL to coaelesce with the Sn63 Solder paste? How reliable is t

Washing of Misprinted PCBs

Electronics Forum | Thu Aug 27 02:55:11 EDT 2009 | smtirl

Alloy is Sn/Pb on a HASL finish. Standard no-clean flux reflowed in Nitrogen.

Fiducials

Electronics Forum | Tue Jul 06 11:58:44 EDT 2010 | baildl632

What type of finish are the PCB's? HASL, tin immersion, silver immersion,........we've seen all the above problems with HASL finished boards. Usually either reheating w/ a soldering iron or "burnishing" with a scotch brite pad has worked for us.

Tin HASL finish soldering problems

Electronics Forum | Tue Sep 14 10:10:39 EDT 2010 | teamcanada

We are having an issue with a PCB supplier. Their Tin HASL layer seems to be the problem. We have triedworking with them to correct their process. What seems to have helped is lowering their temperature of the Tin dip from 540 F to 510 F.We still ha

HASL Plating Thickness

Electronics Forum | Tue Jul 27 07:18:44 EDT 2004 | Nippy

How does the HASL finish and stencil match ? I have seen ocasions on fine pitch devices where the HASL can protrude into the stencil aperture either pulling paste down on the snap off or completely blocking the aperture and getting no paste.

Can the old datecode Entek PCB be converted to HASL ?

Electronics Forum | Thu Jul 05 11:14:04 EDT 2001 | caldon

We can offer two ways. We have a process control tool for OSP boards to validate the finish......but the dates yer talking may be best to take Daves F suggestion. NOW as far as the HASL finish goes...We may have your answer. We can Chemically revers

piercing of test vias at ICT

Electronics Forum | Thu Nov 14 05:45:51 EST 2002 | Jon O'Connell

Has anyone had experiences of ICT test fixtures actually damaging the PCB boards - typically when they have moved away from HASL finish to OSP. I would also like to hear more about any specific issues seen at ICT for non HASL pcb finishes thanks -


hasl finished searches for Companies, Equipment, Machines, Suppliers & Information

Selective soldering solutions with Jade soldering machine

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
Selective soldering solutions with Jade soldering machine

Benchtop Fluid Dispenser
Equipment Auction - Eagle Comtronics: Low-Use Electronic Assembly & Machining Facility 2019 Europlacer iineo + Placement Machine  Test & Inspection: Agilent | Tektronix | Mantis Machine Shop: Haas VF3 | Haas SL-20 | Mult. Lathes

Best Reflow Oven
PCB separator

Find a wide selection of nozzles, solder materials, storage solutions and more at SALESCON