Re: Altera PQFP240 Solderability

Electronics Forum | Tue Apr 14 09:01:36 EDT 1998 | Justin Medernach

| We are having some difficulty soldering a 240 pin Altera device. We use Alpha WS-609, a very generic profile for that solder paste, and a 6 mil stencil with laser cut apertures (1:1 ratio). This is a 20 mil pitch device (aperture size is 10 mils X

Gold plated board, with csp's and 0603 with no clean apetures

Electronics Forum | Thu Sep 26 20:43:51 EDT 2002 | davef

"OK. If the connection doesn't look like I expect it to look, how do I know that the metallurgy is correct?" Comments are: * There are no pictures that will get you though this. * You should expect that gold that is dissolved in Pb/Sn solder to make

Re: Altera PQFP240 Solderability

Electronics Forum | Thu Apr 16 13:50:49 EDT 1998 | Lou

| We are having some difficulty soldering a 240 pin Altera device. We use Alpha WS-609, a very generic profile for that solder paste, and a 6 mil stencil with laser cut apertures (1:1 ratio). This is a 20 mil pitch device (aperture size is 10 mils X

Re: Altera PQFP240 Solderability

Electronics Forum | Thu Apr 16 13:47:36 EDT 1998 | Lou

| We are having some difficulty soldering a 240 pin Altera device. We use Alpha WS-609, a very generic profile for that solder paste, and a 6 mil stencil with laser cut apertures (1:1 ratio). This is a 20 mil pitch device (aperture size is 10 mils X

Re: Gold boards

Electronics Forum | Thu Jul 02 15:23:15 EDT 1998 | Justin Medernach

| | I'm having a problem getting good reflow on gold sufaced boards. The profile looks good and I have adjusted it both hotter and colder and adjusted the various times ( soak, reflow ) to no avail. What realy gets me Is that a month ago we built som