Electronics Forum | Thu Jan 14 13:25:53 EST 1999 | Chrys
| Hi Folks. Has any Process Engineer here done a complete evaluation or controlled experiment for VOC-FREE Flux? Our goal here at CEBUKid, Inc. is to implement a VOC-FREE process. We have all the necessary (OPTIFLUX) spray equipment, and we're cur
Electronics Forum | Mon Feb 22 16:39:33 EST 1999 | C.K.
| | Hi Folks. Has any Process Engineer here done a complete evaluation or controlled experiment for VOC-FREE Flux? Our goal here at CEBUKid, Inc. is to implement a VOC-FREE process. We have all the necessary (OPTIFLUX) spray equipment, and we're c
Electronics Forum | Tue Dec 01 07:24:44 EST 1998 | Earl Moon
| Hi folks , | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspection
Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty
| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec
Electronics Forum | Tue Nov 10 09:45:52 EST 1998 | Scott McKee
| We are currently in the process of purchasing a new low volume SMT line. Based on our research, Quad and Mydata seems to best fit our applications. Has anyone used both equipment and experience the pro and cons of each machine? Thanks in advance fo
Electronics Forum | Mon Nov 02 22:57:02 EST 1998 | Kelly Gossman
Micheal, What does your profile look like for the wave? What profile does your flux say you need? My guess is it is not your profile, our testing with solder balls found that the mask on the boards was the largest contributor to solder balls. Wha
Electronics Forum | Mon Oct 19 14:24:06 EDT 1998 | Justin Medernach
| | | | | | | | It seems like most people want to X-Ray their BGAs. We're going to start doing a lot more of them and need to consider X-ray, too. | | | | | | | | Q: Do most people/companies X-ray everyBGA or do they just do SPC? | | | | | | | | Q:
Electronics Forum | Tue Sep 22 13:14:27 EDT 1998 | Chrys
| We are getting into a lot of double sided boards offlate. Our customer is loading a lot of RNETS, Diodes ( MINLS, SOT23s and other 2 leaded diodes ). We are processing it through a traditional glue process and wave soldering the SMT parts along wit
Electronics Forum | Tue Sep 22 12:25:31 EDT 1998 | Chrys
| | Hi Jacqueline! | | Do these joints that you're having problems with happen to be on fine pitch solder joints? Are the fillets staying attached to the foot and separating from the pads cleanly? | | If that is true, are there many vias concen
Electronics Forum | Tue Sep 15 07:54:42 EDT 1998 | Rob Fischer
| | I am running composite fixtures on my wave solder machine and after about 500 passes each (1 month)they are showing serious signs of wear in that the composite surface is bubbling up and glass fibers are also starting to show. | | The problem h