Electronics Forum | Wed Aug 12 14:39:09 EDT 1998 | Mike C
| Have an SRT w/preheat, 18 layer board all copper, 456 BGA needs to be removed and replaced. The manufacturer is Chip Express and during reflow it warps up or down. Causing either opens or shorts on the corners. I was using gel flux with multiple
Electronics Forum | Thu May 20 19:11:48 EDT 1999 | Earl Moon
| | hello...can somebody help me regarding the POPCORN at Reflow. What is this POPCORN at reflow, what it looks like, its cause and corrective action if there is... | | | | your help is greatly appreciated...thanks | | | | omat marasigan | | | Deo
Electronics Forum | Tue Nov 01 15:26:43 EST 2005 | GS
Is it this your first experience of C-CGA RWK ? In order to approach a RWK of this kind of pakage it requires a capable process and clear operating procedure. In the past, the company who I use to work for, we rwkd plenty of this kind of CCGA. Earl
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830