SMTnet Express, May 26, 2016, Subscribers: 24,776, Companies: 14,803, Users: 40,361 Influence of Salt Residues on BGA Head on Pillow (Hip) J. Servin, P. Gomez, M. Dominguez, A. Aragon; Continental Corporation The oxide layers are known as wetting
SMTnet Express, May 3, 2018, Subscribers: 31,026, Companies: 10,927, Users: 24,677 Hot Air vs. IR BGA Rework Stations Dennis O'Donnell; Precision PCB Services, Inc Hot Air and IR are the two main types of rework stations used by OEMs and PCB
Head-in-Pillow BGA Defects Head-in-Pillow BGA Defects. Head-in-pillow (HiP), also known as ball-and-socket, is a solder joint defect where the solder paste deposit wets the pad, but does not fully wet the ball. This results in a solder joint