Hello, I have been recently bringing a new RoHS wave sold... - Aug 25, 2009 by pb wave
Trapped moisture can be a problem, and one standard recommen... - Aug 25, 2009 by davef
Many thanks for the reply. However, surely because it's ... - Sep 08, 2009 by pb wave
We think the idea is to avoid boiling-off the moisture and l... - Sep 08, 2009 by davef
We understand that you have boards in production that you ne... - Sep 09, 2009 by davef
You mention silver pcbs - baking will accelerate oxidation/t... - Sep 09, 2009 by MikeS