I am currently experiencing major issues when printing fine ...
- May 19, 2010
by
rem
How thick is the stencil?
Also what type of paste?
We ha...
- May 19, 2010
by
Stephen
What is the area ratio for the aperture? What size paste ar...
- May 20, 2010
by
MikeS
I just got word from my board designer that the actual pad s...
- May 20, 2010
by
rem
I believe industry standard is 1/2 pitch for fine pitch devi...
- May 20, 2010
by
MikeS
Thanks I will give this a shot.
...
- May 21, 2010
by
rem
A guideline that I use agrees with MikeS: For 20mil pitch, a...
- May 24, 2010
by
DeanM
Yes, I use Indium Mesh 3. I have a re-cut stencil on the way...
- May 25, 2010
by
rem