Hello all. I need you advice and opinion on my problem wi... - May 23, 2014 by Edri
Hello, these pads look so clean.....I am not sure you had... - May 23, 2014 by Evtimov
Agree with previous comment regarding possible head-in-pillo... - May 23, 2014 by RBoguski
I don't see any visuals that make me think of black pad phen... - May 23, 2014 by Hegemon
Hi Evtimov. 1. yes both part and the process are lead free/... - May 23, 2014 by Edri
Hi Hege. I was not also too confident with the black pad ... - May 23, 2014 by Edri
Just from the look of things (a picture) I would first guess... - May 28, 2014 by Hegemon
Edri, if the profile is good for this part and everything... - May 29, 2014 by Evtimov
whats the type of paset and the type of profile you're runni... - May 29, 2014 by Chris