Recently we facing the Golden finger reject due to contamina... - Nov 13, 2017 by slah6678
Preemptively you can apply Kapton tape to protect the gold f... - Nov 13, 2017 by Steve Thomas
Determine the origin of the solder * Sloppy paste printi... - Nov 13, 2017 by davef
Hi, thanks for reply. Kapton tape is costly and it may cr... - Nov 13, 2017 by slah6678
Hi David, thanks for reply We did doing some study, most p... - Nov 13, 2017 by slah6678
If you think the problem is occurring in the box and it is w... - Nov 14, 2017 by davef
Yes, thanks for bringing up that point, DaveF. All polyimide... - Nov 14, 2017 by Steve Thomas
You don't clean contaminated gold fingers so much as you rep... - Nov 15, 2017 by Stephen