Views: 11935
Hi to all experts, Can anyone advice us what solder alloy t... - Nov 23, 2017 by myke_SMT
Help me understand your issue better ... Are you looking to:... - Dec 07, 2017 by davef
Hi Dave, thanks for the response. * Improve your product... - Dec 10, 2017 by myke_SMT
Hi! You can choose low-temperature solder paste. The low-te... - Jun 18, 2019 by Aite
REL alloys from Aim solders maybe worth looking into for thi... - Jun 21, 2019 by BLT Circuit Services Ltd
Can you please tell us which components cracked? Component t... - Jun 24, 2019 by sssamw
Hi I have solved the issue. The component cracking are the b... - Jul 25, 2019 by myke_SMT
We use SNPb for such applications (PCBA for aircraft). We tr... - Aug 03, 2019 by Alexey
Is there any other competitor to REL solder paste? ... - Sep 03, 2019 by Reckless
There are multiple solder alloy options and we have tested m... - Sep 05, 2019 by SMTA-Richard SMTA
There are competitors to REL solder alloys from AIM. Tin-C... - Sep 05, 2019 by SMTA-Tony SMTA