Hello! Do you have a better stencil design to reduce the lar... - May 06, 2019 by SMTA-Rogers SMTA
There are quite a few papers out there on the subject. Just ... - May 06, 2019 by Steve Thomas
I have personally never seen a reflow profile change reduce ... - May 07, 2019 by Sr. Tech
Probably just means you started out with an optimal profile.... - May 07, 2019 by Steve Thomas
Hi, You can work on improving stencil design, having the p... - May 09, 2019 by CW Solderking
Dear Steve, Thanks for your feedback in our experience add ... - May 27, 2019 by SMTA-Rogers SMTA
Dear Sr.Tech, We tried to adjust the soak time and TAL time... - May 27, 2019 by SMTA-Rogers SMTA
Dear Steve, We already to do some DOE of reflow profile, bu... - May 27, 2019 by SMTA-Rogers SMTA
Dear CW, Yes, we also tested many different brands and mode... - May 27, 2019 by SMTA-Rogers SMTA
Solder paste flux is main contributor, Lead termination chem... - May 28, 2019 by josh
Contributors in order of importance: 1. PCB design - if you... - May 30, 2019 by Evtimov