We recently installed a new solder wave machine, The spray f... - Mar 06, 2023 by Pratyeka
We use Nitrogen to inert the Selective Solder, as well as sp... - Mar 07, 2023 by ProcEng1
any advantages over other nitrogen systems, like cost, maint... - Mar 07, 2023 by Pratyeka
Prior to the Generators, we bought tanks of N2. As long as... - Mar 07, 2023 by ProcEng1
fluxer requires normal shop pressure, around 100psi. Thanks ... - Mar 07, 2023 by Pratyeka
The onsite generator drops approx. 30psi from the input. We... - Mar 07, 2023 by ProcEng1
Sounds right, our actual pressure in the system is 120psi, t... - Mar 07, 2023 by Pratyeka
What purity? To get 99.999% pure you will need dewers of liq... - Mar 07, 2023 by Stephen
we don't have a nitrogen generator installed yet. The solder... - Mar 08, 2023 by Pratyeka
Agreed. If it's just a means of propulsion/ atomization the ... - Mar 08, 2023 by ProcEng1
For fun ask the sales guy where they came up with that numbe... - Mar 08, 2023 by Stephen