We are investigating purchasing boards off-shore (Topsearch). Part of their process is to punch the matrix instead of router them. These boards are mixed technology. Is anyone aware of difficulity processing punched boards? Thanks, Mike

reply »

Earl Moon

#13440

Re: Punched vs, Routered PCB's | 19 November, 1998

| We are investigating purchasing boards off-shore (Topsearch). Part of their process is to punch the matrix instead of router them. These boards are mixed technology. Is anyone aware of difficulity processing punched boards? | Thanks, | Mike | Big tooling charges to make dies. Not to be used with MLB's of any sophistication. Used mostly with "cheap and dirty" PCB's, etc.. Re-sharpen or re-tool dies as required.

Earl Moon

reply »

Kallol Chakraborty

#13441

Re: Punched vs, Routered PCB's | 22 November, 1998

| | We are investigating purchasing boards off-shore (Topsearch). Part of their process is to punch the matrix instead of router them. These boards are mixed technology. Is anyone aware of difficulity processing punched boards? | | Thanks, | | Mike | | | Big tooling charges to make dies. Not to be used with MLB's of any sophistication. Used mostly with "cheap and dirty" PCB's, etc.. Re-sharpen or re-tool dies as required. | | Earl Moon | I completely agree with Earl. But I am not sure if you are talking about flex, rigid or rigid/flex combo . Usually for flex, most of the time we have no choice but to use die which is very expensive to re-sharpen (potential failure mode - dimension tol., special space, rev control required for the die itself ).

For MLB it could cause severe edge delamination /separation and is very hard to punch over 60 mil thick > 3 lyr with gnd /pwr plane (most of the mixed has sheilding). I guess I am just repeating what Earl has said earlier.

It would be nice to ask them for sub-ing it out for scoring as sometimes it is hard to route (SS or DS). I am pretty sure that there are a lot of scoring / routing house who could do a pretty good job and charge dirt cheap at the same time. Also depending on the capacity and need, you could ask them to buy any one of them - Accuscore for scoring or a used routing machine -