Hello All, I've got a little problem here. I have a 456 ba...
- May 14, 2002
by
RDR
Maybe the issue is not a proper rework method. Your shorts ...
- May 14, 2002
by
davef
Good point, I am preheating for 90 sec to a temp of 170 C. (...
- May 15, 2002
by
RDR
2 suggestions -
Get a good scope - at least a 4X, but mor...
- May 22, 2002
by
I use the exact same paste flux that we use in our solder pa...
- May 27, 2002
by
Reworkman