Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I have some finished boards that I have concluded have "blac...
- Aug 21, 2003
by
adlsmt
Do some push / pull testing. Typically with black pad, you ...
- Aug 21, 2003
by
Justin Medernach
You have one option: Take the boards to the fabricator that...
- Aug 21, 2003
by
davef
Well, for some reason the board house will pay for the board...
- Aug 21, 2003
by
adlsmt
Well after reading all kinds of stuff about this I still que...
- Aug 21, 2003
by
adlsmt
Ask your supplier for a corrective active and failure analys...
- Aug 22, 2003
by
davef