I have a pad layout that has .010" dia. with .010" spacing.
...
- Apr 03, 2006
by
Sr. Tech
Sounds a little like 2" O.D. pipe with 1" wall thickness.
...
- Apr 03, 2006
by
10mil square apertures should be ok with your 4mil stencil.
...
- Apr 04, 2006
by
I have used a .013" square under these conditions.
Limite...
- Apr 04, 2006
by
RDR
I did the apertures 1:1 using an Invar foil material.