Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 9150
Is there a way or process to use the screen printer to put s...
- May 14, 2010
by
Armando_Gomez
Search "paste in hole" or "intrusive reflow"
...
- May 14, 2010
by
Sr. Tech
I worked with a customer about 2 years ago on a process simi...
- May 15, 2010
by
DEKHEAD
We do a lot of intrusive reflow. It works very well but the ...
- May 18, 2010
by
Derek