Hi guys,
Whats actually Delta T ?
As i know,its applic...
- May 18, 2013
by
kumar
Delta T is the temperature difference between the lowest and...
- May 20, 2013
by
JAX
Hi there....
Appreciate your info on this.As mentioned,th...
- May 20, 2013
by
kumar
I don't get it...
Who cares if the zones on your oven are...
- May 20, 2013
by
JAX
Well, you wouldn't want 100 deg difference from zone to zone...
- May 20, 2013
by
Hegemon
Thanks to everyone for your answers...
Delta T represents...
- May 20, 2013
by
kumar
Delta-T in reflow generally means 2 things - difference in t...
- May 21, 2013
by
Hussman
> Thanks to everyone for your answers...
>