Hello Folks,
I am getting a Passaat SMRO-0406 reflow mach...
- Dec 09, 2014
by
Sreejith
Thanks for your reply!! But i dont understand the 300 degree...
- Dec 10, 2014
by
Sreejith
The 300 degrees is the temperature as measured at the sensor...
- Dec 10, 2014
by
JimPat
Hello,
yes you are absolutely correct. I agree with your ...
- Dec 10, 2014
by
Sreejith
The longer the oven, the better. You will have much more cap...
- Dec 11, 2014
by
Evtimov
Hello Sir,
Thanks for your reply. i just got a mail from ...
- Dec 11, 2014
by
Sreejith
ALso, coming to the convection the DIMA service group said :...
- Dec 11, 2014
by
Sreejith
Hello,
So in short, i wanted to know.. for 8 zones i gues...
- Dec 11, 2014
by
Sreejith
If you have a chance ask them to bring in one of your produc...
- Dec 11, 2014
by
Evtimov
why all people speak only the temperatur? the speed convoyor...
- Dec 22, 2014
by
ben
What do you mean by solder in ROHS. Can you please explain m...
- Dec 22, 2014
by
Sreejith
Hello,
Also I wanted to tell you. I decided to go with a ...
- Dec 22, 2014
by
Sreejith
Sounds like your volumes are pretty low. Pick and Place is ...
- Dec 23, 2014
by
JimPat