Hi All, Currently im seeing a cold solder/ poor wetting un... - Oct 19, 2016 by Thanesh
You say, "... re-flow profile temperature, the peak temperat... - Oct 20, 2016 by davef
Looking at your picture I'm not sure you have a wetting prob... - Oct 21, 2016 by SweetOldBob
Dear Thanesh, did You alrady solved issue? We are facing sam... - Sep 15, 2017 by Kubabel
An assembly with this improperly solder joints will have fun... - Sep 16, 2017 by TheBond
Besides the good advises above, I will add my observation. Y... - Sep 18, 2017 by Evtimov
Thank You for these hints, we´ve checked whole temp. profile... - Sep 19, 2017 by Kubabel
SEM Lab, Inc. supports this type of analysis. Please see se... - Sep 20, 2017 by EdHare
Thank You! I will try to go in touch with them... ... - Sep 21, 2017 by Kubabel