Parts are falling off on first side when reflowing second s... - Oct 31, 1999 by
Do both sides of that board contain larger IC's and other l... - Oct 31, 1999 by
I suggest tow more ways: 1. try to differ the temperaturte ... - Nov 01, 1999 by
I suggest tow more ways: 1. try to differ the temperaturte ... - Nov 01, 1999 by
Without a detailed description of the suspect parts It is d... - Nov 01, 1999 by
Assuming you are using Sn63/Pb37 solder paste, have you tri... - Nov 06, 1999 by Gary Moravchik
Gary: This could be messy is some applications, because Bi... - Nov 09, 1999 by davef
Pat Copeland