Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 731
What is the proper storage and shelf life after washing a PC...
- Oct 13, 2021
by
Larry Kobriger
"We sometimes have to pull the boards off the line ...
- Oct 14, 2021
by
dontfeedphils
The best shelf life for OSP is run both sides the same day t...
- Oct 14, 2021
by
Stephen
OSP is there to keep the copper from oxidizing. Once you was...
- Oct 14, 2021
by
SMTA-64387687
SMTA