Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3459
hi, I have supplied 100 kg Solder Rods 63/37 to my customer... - Jun 21, 2022 by Vopasha INC
Are they applying a dross reducing powder, like what you wou... - Jun 21, 2022 by ProcEng1
No. They are not using any dross reducer. I ... - Jun 21, 2022 by Vopasha INC
hi, Enclosed herewith images of mud like dross. ... - Jun 21, 2022 by Vopasha INC
I received an email from the OP and I will not be connecting... - Jun 21, 2022 by ProcEng1
Any Reply to this Photos or any update ... - Jun 25, 2022 by Vopasha INC
Hello ! I got exp only with leadfree HASL, but maybe the sa... - Jul 02, 2022 by madisreivik