Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi, We are placing (+) & (-) terminals in SMT. We have just... - Apr 13, 2003 by
Just some more info: PCB is HAL finished we are using Sn63... - Apr 13, 2003 by
Consider: * Sn has a higher melting point than Pb. So the l... - Apr 14, 2003 by davef
Hi Dave, thanks! The peak temp on the terminal device is ... - Apr 16, 2003 by
First thing to try is get the solder connection hotter. 210... - Apr 17, 2003 by davef
yukim