#74851

Solderability problems with gold plated PCB's | 9 November, 2015

Hi guys,

we have a problem and I hope something can give nme some new information. We have big solderability problems with a gold plated board. We changed the paste already, but there is no improvement.

Could the Vapor phase Technology cause the problems?

Thanks

reply »

#74864

Solderability problems with gold plated PCB's | 11 November, 2015

Could you give us more details. Picture, profile, solder paste ...?

reply »

#74870

Solderability problems with gold plated PCB's | 12 November, 2015

IPC J-STD-003. Solderability Tests for Printed Boards